Subcritical crack growth of Ti-6Al-4V at room temperature under high stress-ratio loading
β Scribed by J.P Thomas
- Book ID
- 114388597
- Publisher
- Elsevier Science
- Year
- 1998
- Tongue
- English
- Weight
- 312 KB
- Volume
- 39
- Category
- Article
- ISSN
- 1359-6462
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
The evolution of intergranular lattice strains in a textured, forged bar (Bar) sample of the a Γ b titanium alloy Ti-6Al-4V has been characterised using in situ X-ray diffraction. A two-phase elastic-plastic self-consistent (EPSC) model has been developed to rationalise the results. Of the orientati
Relaxation behavior of residual stress in a shot-peened titanium alloy, Ti-6Al-4V subjected to fretting fatigue was investigated at room and elevated temperatures. Constant amplitude fretting fatigue tests were conducted at several maximum stress levels, Ο max ranging from 333 to 666 MPa with a stre