๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Study on the fracture process of aluminium under tensile creep test

โœ Scribed by M. A. Soliman; N. Kinawy; M. M. Eleiwa


Publisher
Springer
Year
1986
Tongue
English
Weight
139 KB
Volume
5
Category
Article
ISSN
0261-8028

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Influence of the Dispersoid Material and
โœ Univ.-Prof. Dr.-Ing. E. El-Magd; Assistant Prof. Y. Ismail; Dr. G.-J. Brockmann; ๐Ÿ“‚ Article ๐Ÿ“… 1997 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 628 KB

## Abstract The effect of small percentages of Al4C3 and Al2O3 in dispersion hardened aluminium on the creep behaviour has been investigated. A comparative study was conducted on the group of AlC3Ol and AlC2O2. These two groups were produced by cold isostatic pressing (CIP), but the second group wa