๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Studies of the degradation of metal-adhesive interfaces with surface analysis techniques

โœ Scribed by D.R. Arnott; A.R. Wilson; A.N. Rider; L.T. Lambrianidis; N.G. Farr


Publisher
Elsevier Science
Year
1993
Tongue
English
Weight
525 KB
Volume
70-71
Category
Article
ISSN
0169-4332

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES