Thermo-mechanical fatigue failure of a s
โœ M. Okazaki; M. Sakaguchi ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 480 KB

Behavior of thermo-mechanical fatigue (TMF) of a single crystal Ni-based superalloy, CMSX-4, was studied, compared with that of isothermal low cycle fatigue (LCF). Strain-controlled TMF and LCF tests of CMSX-4 were carried out under various test conditions, where the experimental variables were stra