๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Structural changes in 12Kh1MF pipe during creep tests

โœ Scribed by E. I. Krutasova; G. M. Novitskaya; G. A. Bologov


Book ID
112388148
Publisher
Springer US
Year
1976
Tongue
English
Weight
827 KB
Volume
18
Category
Article
ISSN
0026-0673

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES