Lattice distortion in γ′ precipitates of
✍
W. Chen; N. Darowski; I. Zizak; G. Schumacher; H. Klingelhöffer; W. Neumann
📂
Article
📅
2006
🏛
Elsevier Science
🌐
English
⚖ 154 KB