Unidirectional (UD) composite laminates based on carbon fibers (CF) and high-performance polyethylene fibers (PEF) were prepared with partially polymerized methyl methacrylate (MMA) at 25ЊC, followed by heating at 55ЊC (well below the softening point of PEF) for 2 h. The viscoelastic behavior of the
Stress-relaxation behavior of unidirectional polyethylene–carbon fibers: PMMA hybrid composite laminates
✍ Scribed by Nirmal Saha; Amar Nath Banerjee
- Publisher
- John Wiley and Sons
- Year
- 1998
- Tongue
- English
- Weight
- 131 KB
- Volume
- 67
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
✦ Synopsis
Unidirectional composite laminates based on carbon fibers (CF) and highperformance polyethylene fibers (PEF) and their hybrids were prepared with partially polymerized methyl methacrylate (MMA) at room temperature, followed by heating at 55ЊC (well below the softening point of PEF, 147ЊC) for 2 h. The stress-relaxation behavior of the composites were determined and analyzed. It was found that at all strain levels the rate of stress relaxation decreased by the loading of CF in CF-reinforced composite laminates (CFRC); however, the reverse behavior was found in the case of PEF-reinforced composite laminate (PEFRC). An interesting observation of the study was that the rate of stress relaxation decreased linearly in two steps in the case of PEFRC, whereas in the case of CFRC, it decreased in a single step. In the case of hybrid composites, the stress relaxation decreases in two steps as in PEFRC. ᭧ 1998
📜 SIMILAR VOLUMES
Unidirectional (UD) composite laminates based on glass fibers (GF) and high-performance polythylene fibers (PEF) were prepared with partially polymerized methyl methacrylate (MMA) at room temperature, followed by heating at 55°C (well below the softening point of PEF) for 2 h. The tensile strength,
Unidirectional (UD) composite laminates based on high-performance polyethylene fibers (PEF) and glass fibers (GF) and their hybrids were prepared with partially polymerized methyl methacrylate (MMA) at room temperature, followed by heating at 55°C (well below the softening point of PEF, 147°C) for 2
Unidirectional (UD) hybrid composite laminates based on glass fibers (GF) and high performance polyethylene fibers (PEF) were prepared with partially polymerized methyl methacrylate (MMA) at room temperature, followed by heating at 55°C (well below the softening point of PEF) for 2 h. The total volu