Stress corrosion testing and data analysis

✍ Scribed by Dr. V. M. Radhakrishnan; Dr. S. Ramakrishna Iyer


Publisher
John Wiley and Sons
Year
1979
Tongue
German
Weight
431 KB
Volume
30
Category
Article
ISSN
0947-5117

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

Experiments have been carried out on structural materials to investigate the effect of pre‐straining on the rupture strength. The effect of sodium chloride on aluminium and stainless steel and that of ammonium hydroxide on brass and copper has been analysed. It hat been found that the rupture strength decreases with increasing pre‐strain. A stress corrosion index has been defined and this index has been found to depend on the initial pre‐strain; a linear relation exists with the percentage of pre‐strain.


πŸ“œ SIMILAR VOLUMES


Corrosion and materials testing
πŸ“‚ Article πŸ“… 1995 πŸ› John Wiley and Sons 🌐 German βš– 158 KB

44073, U.S.A. (nicht jedoch an die VCH Veriagsgesellschaft rnbH!) zu wenden. Die Kosten fur Fotokopien betragen $10.00 fur jeweiis 10 Seiten und $4.00 fur zusatzliche 10 Seiten (US-Office) oder f 7.00 fur 10 Seiten und f 3.00 fur zusatzliche 10 Seiten (UK-Office). Einen Schlussel zu den abgekutzten

Corrosion and materials testing
πŸ“‚ Article πŸ“… 1995 πŸ› John Wiley and Sons 🌐 German βš– 362 KB

USA. [nicht jedoch an die VCH Verlagsgesellschaft mbH!) zu wenden. Die Kosten fur Fotokopien betragen $ 10.00 fur jeweils 10 Seiten und $4.00 fur zusatzliche 10 Seiten (US-Office) oder f 7.00 fur 10 Seiten und f 3.00 fur zusatzliche 10 Seiten (UK-Office). Einen Schlussel zu den abgekurzten Quellenan

Corrosion and materials testing
πŸ“‚ Article πŸ“… 1995 πŸ› John Wiley and Sons 🌐 German βš– 366 KB

Korrosions-und Werkstoffprufung Arbeiten uber mehrere Werkstoff gruppen Eisenmetalle Nichteisenmetalle Corrosion and materials testing Nichtmetallische anorganische Non-metallic inorganic Werkstoff e materials Kunststoffe und andere Metallische Uberziige Metal coatings Plastics and other Comprehensi

Corrosion and materials testing
πŸ“‚ Article πŸ“… 1995 πŸ› John Wiley and Sons 🌐 German βš– 365 KB

Korrosions-und Werkstoff-pNfung Werkstoffe materials Arbeiten iiber mehrere Werk-Comprehensive papers covering organische Werkstoffe organic materials stoffgruppen several materials groups Corrosion and materials testing Nichtmetallische anorganische Non-metallic inorganic Kunststoffe und andere Met