𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Stress Corrosion Susceptibility of Polymeric-Coated Soda-Lime Glass

✍ Scribed by J. E. RITTER JR.


Book ID
110813770
Publisher
John Wiley and Sons
Year
1973
Tongue
English
Weight
254 KB
Volume
56
Category
Article
ISSN
0002-7820

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES