## Abstract The article presents the test results of stress corrosion resistance of explosion welded steelβaluminum elements. The tests were carried out by means of the slow strain rate test (10^β6^ s^β1^) in air and artificial sea water. The following parameters were measured: tensile strength, ti
β¦ LIBER β¦
Stress corrosion cracking of welded joints between dissimilar materials
β Scribed by N. N. Zhagalyak; I. I. Vasilenko; G. V. Karpenko
- Publisher
- Springer
- Year
- 1973
- Tongue
- English
- Weight
- 442 KB
- Volume
- 7
- Category
- Article
- ISSN
- 1573-885X
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Stress corrosion cracking of explosion w
β
M. Czechowski
π
Article
π
2004
π
John Wiley and Sons
π
German
β 281 KB
Possible application of metallized coati
β
A. I. Zyubrik; G. M. Rubinshtein; I. I. Vasilenko
π
Article
π
1973
π
Springer
π
English
β 178 KB
Effect of cracked weld joint and yield s
β
J.Q. Fu; Y.W. Shi
π
Article
π
1996
π
Elsevier Science
π
English
β 403 KB
Introduction of stress functions around
β
Y. Murase; K. Nakagawa; T. Hachiya; S.J. Duan
π
Article
π
1996
π
Elsevier Science
π
English
β 606 KB
The stress concentration around a circular interface crack between two dissimilar elastic planes is analysed in this paper. The constructive algorithm of the group of general stress functions which satisfy the crack boundary conditions is introduced. From that, six analytic solutions are selected to
Corrosion behaviour of soldered joints o
β
Wielage, Bernhard ;MΓΌcklich, Silke ;Grund, Thomas
π
Article
π
2006
π
Springer-Verlag
β 365 KB
Intercrystalline Corrosion Cracking of W
β
B. T. Timofeev; V. A. Fedorova; A. A. Buchatskii
π
Article
π
2004
π
Springer
π
English
β 882 KB