𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Stress corrosion cracking of FeCoBSi metallic glasses in HCl solutions

✍ Scribed by Habib, K


Book ID
123286621
Publisher
Elsevier Science
Year
1994
Weight
275 KB
Volume
31
Category
Article
ISSN
0956-716X

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Heat capacity of metallic glasses FeNi
✍ Takeshi Kanomata; Hideharu Endo; Minoru Kuboki; Hisamichi Kimura; Takejiro Kanek 📂 Article 📅 1994 🏛 Elsevier Science 🌐 English ⚖ 290 KB

The specific heats of Fe72NilsZr10, C072.9Cr17.1Zrlo , Ni78Si10B12 and PdsoSi20 amorphous alloys were measured in the temperature range 77-800 K. The magnetic anomaly of the heat capacity at the ferromagnetic Curie temperature T c was observed for Fe-Ni-Zr alloy, but not for Co-Cr-Zr. The results ar