𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Stress corrosion cracking of AISI 304 and 316 stainless steels in lithiated water at 350°C

✍ Scribed by S.W. Sharkawy; Z. Xia; Z. Szklarska-Smialowska


Publisher
Elsevier Science
Year
1992
Tongue
English
Weight
764 KB
Volume
195
Category
Article
ISSN
0022-3115

No coin nor oath required. For personal study only.