𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Stress corrosion cracking of a BaTiO3 ferroelectric ceramics

✍ Scribed by R.M Wang; W.Y Chu; K.W Gao; W.Y.J Su; L.J Qiao


Book ID
116730261
Publisher
Elsevier Science
Year
2004
Tongue
English
Weight
236 KB
Volume
58
Category
Article
ISSN
0167-577X