๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Stress-corrosion cracking and crevice corrosion in passivable alloys

โœ Scribed by G. Bombara


Book ID
115845829
Publisher
Elsevier Science
Year
1969
Tongue
English
Weight
696 KB
Volume
9
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Stress Corrosion Cracking of Magnesium A
โœ Andrej Atrens; Nicholas Winzer; Wolfgang Dietzel ๐Ÿ“‚ Article ๐Ÿ“… 2011 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 880 KB
Theoretical description of the practical
โœ S. Wang ๐Ÿ“‚ Article ๐Ÿ“… 2005 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 97 KB

Stress corrosion cracking (SCC) from crevice corrosion sites had been found in an experimental work at polarization potential of รพ 200 mV SCE . In that work, an occluded U-bend specimen of Type 316L (UNS S31603) stainless steel was used. The testing was done in sodium chloride (NaCl) solution. Based