๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Specific heat of neutron irradiated graphite

โœ Scribed by S. Mrozowski; A.S. Vagh; K. Kamiya


Publisher
Elsevier Science
Year
1972
Tongue
English
Weight
129 KB
Volume
10
Category
Article
ISSN
0008-6223

No coin nor oath required. For personal study only.

โœฆ Synopsis


Neu! Y&Z). In extension of the work of Delhaes and Hisiyama* measurements of specific heat in the range @5-5ยฐK were carried out on soft carbons heattreated in the range 6~)-1600ยฐC. A largp increase in the linear component with decrease in HTT is observed as well as also in the cubic component. The specific heat peak at 0*65"K is found to be present irrespective of the origin of the carbon, becoming quite pronounced for low heattreatment.


๐Ÿ“œ SIMILAR VOLUMES


81. Low temperature specific heat of neu
โœ S Mrozowski; S Orzeszkof; A.S Vagh ๐Ÿ“‚ Article ๐Ÿ“… 1973 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 121 KB

The specific heat of glassy carbon was investigated in the temperature range of 0\*44-4\*5"K. The specific heat follows a relation C = aT3+ yT, with y going through a ma~mum and a! increasing with increase in heattreatment temperature. On the average the cubic specific heat term is about the same as

Thermal conductivity of neutron-irradiat
โœ R.J. Price ๐Ÿ“‚ Article ๐Ÿ“… 1975 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 402 KB

The thermal conductivity of neutron-irradiated reactor-grade graphites made from needle coke (H-327), Gilsocoke (H-328), and isotropic petroleum coke (H-451) was measured between 22 and 800ยฐC. Irradiation temperatures were between 600 and 16OO"C, and fast neutron fluences ranged up to lO22 n/cm\* (E

Neutron irradiation and surface homogene
โœ D.A Cadenhead ๐Ÿ“‚ Article ๐Ÿ“… 1964 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 453 KB

The possibility of assessing by means of sorption techniques the surface damage due to neutron irradiation of graphitic materials has been investigated. Samples of a graphitized carbonblack (S6-D3) were subjected to an integrated neutron flux of 2.6 x 10%/cm2 and 4.7 X 10%/cmz of both thermal and fa