Specific features of rhenium-alloyed single-crystal nickel superalloys

โœ Scribed by E. N. Kablov; N. V. Petrushin; M. B. Bronfin; A. A. Alekseev


Book ID
110185765
Publisher
SP MAIK Nauka/Interperiodica
Year
2006
Tongue
English
Weight
434 KB
Volume
2006
Category
Article
ISSN
0036-0295

No coin nor oath required. For personal study only.