Assessment of corrosion-induced damage a
✍
Shaikh Faiz Uddin Ahmed; Mohamed Maalej; P. Paramasivam; Hirozo Mihashi
📂
Article
📅
2006
🏛
John Wiley and Sons
🌐
English
⚖ 349 KB
## Abstract This paper reports the results of an experimental program on the effect of steel loss and corrosion induced‐damage (cracking, delamination, spalling, etc.) on the post‐corrosion flexural response of reinforced concrete beams incorporating supplementary cementing materials (fly ash, slag