Films of isotactic polystyrene (ips) were quenched at different temperatures (0, 40, ZOOOC). Wide-angle X-ray diffractograms, differential scanning calorimetry (DSC) and Fourier transform infrared spectroscopy (FTIR) show that the three samples are amorphous; slight differences were found in the den
Solvent-induced crystallization of isotactic polypropylene in cyclohexane at different temperatures
✍ Scribed by V. Vittoria
- Publisher
- Elsevier Science
- Year
- 1991
- Tongue
- English
- Weight
- 323 KB
- Volume
- 32
- Category
- Article
- ISSN
- 0032-3861
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Temperature dependence of ~H spin-lattice, Tt (H), and spin-spin, T2(H ), relaxation times of isotactic polypropylene samples with different microtacticity was investigated. The samples were crystallized at high temperature (155°C) for a long time (200hr). The sample with high microtacticity (mmmm =
## Abstract Melt history, pressure, and crystallization temperature are three variables that may be used to vary spherulite size in polymer systems. In this study, bulk polypropylene samples were given various melt treatments and then isothermally crystallized under constant pressure. Spherulite si
## Abstract Nach dem Ausschalten der Erregerspannung, die an eine in Resonanz schwingende Quarzplatte gelegt war, wird das Abklingen des piezoelektrischen Stromes in Benzin und anderen Flüssigkeiten in Abhängigkeit von der Temperatur gemessen, um Viskositätsänderungen bei Ultraschall‐Frequenzen zu