Simultaneous sulphidation and oxidation of Fe-25 wt.%Cr and Silicon-containing Fe-25 wt.%Cr alloys in H2H2OH2S gas mixtures at high temperatures

✍ Scribed by C.R. Wang; W.Q. Zhang; R.Z. Zhu