𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Shear Band Formation in Fe–Cr–Mo–V–B–Si Amorphous Alloy under Nanoindentation

✍ Scribed by M. N. Vereshchagin; S. N. Dub; V. G. Shepelevich; O. M. Ostrikov


Book ID
111588036
Publisher
SP MAIK Nauka/Interperiodica
Year
2004
Tongue
English
Weight
131 KB
Volume
45
Category
Article
ISSN
0021-8944