Sensitivity of acoustic emission for the detection of stress corrosion cracking during static U-bend tests on a 316L stainless steel in hot concentrated magnesium chloride media
✍ Scribed by F. Ferrer; E. Schille; D. Verardo; J. Goudiakas
- Book ID
- 110343076
- Publisher
- Springer
- Year
- 2002
- Tongue
- English
- Weight
- 326 KB
- Volume
- 37
- Category
- Article
- ISSN
- 0022-2461