The formation rate of carbonaceous mesop
โ
Y Yamada; S Oi; H Tsutsui; E Kitajima; M Tsuchitani; H Kakiyama; H Honda
๐
Article
๐
1975
๐
Elsevier Science
๐
English
โ 129 KB
Abstr anthracene chars heat treated between 500 and 1200ยฐC is developped and applied to d.c. electrical conductivity, paramagnetic susceptibility and apparent density. An inhomogeneous process for the carbonization is proposed, in agreement with recent results on the structure of these chars. acts 3