✦ LIBER ✦
Selection of methods for etching carbides in MAR-M509 cobalt-base superalloy and acquisition of their images
✍ Scribed by Janusz Szala; Agnieszka Szczotok; Janusz Richter; Jan Cwajna; Adolf Maciejny
- Book ID
- 113779924
- Publisher
- Elsevier Science
- Year
- 2006
- Tongue
- English
- Weight
- 990 KB
- Volume
- 56
- Category
- Article
- ISSN
- 1044-5803