𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Second generation columnar grain nickel-base superalloy: Cetel, A. D. and Duhl, D. N. Proc. Conf. Superalloys 1992, Champion, Pennsylvania, USA, 20–24 Sept. 1992 (The Minerals, Metals & Materials Society, 420 Commonwealth Dr, Warrendale, PA 15086, USA) 1992 pp 287–296


Book ID
107891736
Publisher
Elsevier Science
Year
1993
Tongue
English
Weight
189 KB
Volume
15
Category
Article
ISSN
0142-1123