Role of second phases in the stress corrosion cracking of a nickel–aluminium bronze in saline water

✍ Scribed by Stéphanie Fonlupt; Bernard Bayle; David Delafosse; Jean-Loup Heuze


Book ID
116384309
Publisher
Elsevier Science
Year
2005
Tongue
English
Weight
879 KB
Volume
47
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.