✦ LIBER ✦
Refractory Carbides || Electron-Fractographic Study of the Fractures in Zirconium Carbide after Tensile Testing in the Range 20–2000°C
✍ Scribed by Samsonov, Grigorii V.
- Book ID
- 120227939
- Publisher
- Springer US
- Year
- 1974
- Weight
- 387 KB
- Category
- Article
- ISBN
- 1468485989
No coin nor oath required. For personal study only.