Recovery of point defects in iron after
โ
L.J. Cuddy
๐
Article
๐
1968
๐
Elsevier Science
โ 550 KB
High-purity iron was severely deformed at 77ยฐK by rolling or drawing under liquid nitrogen. Changes in electrical resist.ivity were used to measure the recovery during isochronal and isothermal anneals in the temperature range llO-520ยฐK. A sharp recovery stage was observed at 211ยฐK for which t,he ac