An annealing study was performed on cold-rolled IC-218 alloy (an advanced form of nickel aluminide) with a reduction of 607. During isochronal annealing for 10 min, a hardness maximum was found at 475 C; this was due to reordering, as confirmed by DSC analysis. When the annealing temperature was rai
✦ LIBER ✦
Recovery and recrystallization of cold-rolled nickel in magnetic fields
✍ Scribed by Günter Neite; Eckhard Nembach
- Publisher
- Elsevier Science
- Year
- 1982
- Weight
- 228 KB
- Volume
- 52
- Category
- Article
- ISSN
- 0025-5416
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Recovery and Recrystallization of 60%-Co
✍
Lin, Yijian ;Wu, Xingfang ;Ke, Jun ;Cahn, R. W.
📂
Article
📅
1998
🏛
John Wiley and Sons
🌐
English
⚖ 395 KB
In Situ EBSD Investigation of Recrystall
✍
Anne-Laure Helbert; Wei Wang; François Brisset; Thierry Baudin; Richard Penelle
📂
Article
📅
2011
🏛
John Wiley and Sons
🌐
English
⚖ 613 KB
## Abstract The microstructure of partially annealed and additionally rolled 1050 aluminum alloy of commercial purity was monitored using FEG/EBSD in situ heating experiments in order to understand the preferential growth of Cube‐oriented grains. A fast reorganization of the deformation sub‐structu
The influence of recovery and recrystall
✍
B.F. Rothenstein; O.F.G. Aczel
📂
Article
📅
1970
🏛
Elsevier Science
🌐
English
⚖ 168 KB
The formation of (110)[001] recrystalliz
✍
Hsun Hu
📂
Article
📅
1960
🏛
Elsevier Science
⚖ 490 KB
Physical and Numerical Simulation of Col
✍
Christoph Heering; Xiaoli Li; Markus Bambach; Gerhard Hirt
📂
Article
📅
2010
🏛
John Wiley and Sons
🌐
English
⚖ 664 KB
ChemInform Abstract: Impact of Magnetic
✍
Dmitri A. Molodov
📂
Article
📅
2008
🏛
John Wiley and Sons
⚖ 15 KB