Recognition of weld defects in x-ray inspection film by image processing (In Japanese) : Suga, Y Journal of JSNDI, Vol. 44, No. 11, pp. 869–874 (Nov. 1995)


Book ID
108042549
Publisher
Elsevier Science
Year
1996
Tongue
English
Weight
127 KB
Volume
29
Category
Article
ISSN
0963-8695

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Development of the automatic system for
📂 Article 📅 1996 🏛 Elsevier Science 🌐 English ⚖ 165 KB

This paper presents a three-dimension radiograph detector for inspecting the location of weld defects and their sizes, including spilly place, aircavity, slag inclusion, uncomplete weld of edge joint. Confirmed by the actual dissection of weld, the testing results show that the absolute error is les