Ultrafine cobalt powders have been prepared by the freeze-drying method and supported cobalt catalysts have been prepared by a new freeze-drying immersion method. The results of XRD and SEM showed that the precursors were amorphous and most were massive with a size range of 2-5 ยตm. In the cobalt pow
Reactive deposition of ultrafine cobalt powders
โ Scribed by C. Q. Cui; J. Y. Lee; T. C. Tan
- Publisher
- Springer
- Year
- 1994
- Tongue
- English
- Weight
- 587 KB
- Volume
- 29
- Category
- Article
- ISSN
- 0022-2461
No coin nor oath required. For personal study only.
โฆ Synopsis
The particle size distributions of cobalt powders prepared by reactive deposition were examined and correlated with the deposition condition. In reactive deposition, a Co (OH)2 colloid layer was formed at the electrode surface upon reduction of dissolved oxygen. The colloid layer accelerated the decrease in interfacial Co 2+ concentration and inhibited crystal growth of the metal, and was therefore instrumental in the formation of fine cobalt particles. The powders from reactive deposition were statistically a factor of two finer and of more uniform size distribution than those from normal electrodeposition. It was found that both the reactive deposition of cobalt powders and the reactive deposition of porous cobalt structures were driven by the same kinetic factors, namely the requirement of maintaining an effective presence of the Co (OH)2 colloid layer at the electrode surface. Hence a similar dependence on deposition conditions for both processes was obtained.
๐ SIMILAR VOLUMES