Quantitative Fractography of Mixed-Mode Fracture in Soda Lime Silica Glass

✍ Scribed by Karthik Gopalakrishnan; John J. Mecholsky Jr.


Book ID
117962653
Publisher
John Wiley and Sons
Year
2012