Quantitative examination of stress corrosion cracking of alloy 600 in high temperature water

โœ Scribed by R. Bandy; D. van Rooyen


Publisher
Elsevier Science
Year
1985
Tongue
English
Weight
699 KB
Volume
86
Category
Article
ISSN
0029-5493

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Stress corrosion cracking and selective
โœ E. Brandl; R. Malke; T. Beck; A. Wanner; T. Hack ๐Ÿ“‚ Article ๐Ÿ“… 2009 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 823 KB

## Abstract Despite a generally good corrosion resistance to tap and industrial water, many brass taps and fittings have failed in the past by stress corrosion cracking (SCC) and selective corrosion (dezincification or preferred removal of a phase). The experimental investigations of the present st