Probabilistic modelling of steam generator tube pitting corrosion

✍ Scribed by Suresh V. Datla; Mikko I. Jyrkama; Mahesh D. Pandey


Publisher
Elsevier Science
Year
2008
Tongue
English
Weight
889 KB
Volume
238
Category
Article
ISSN
0029-5493

No coin nor oath required. For personal study only.

✦ Synopsis


Pitting corrosion is a serious form of degradation in steam generator (SG) tubing of some nuclear stations. The nature and extent of the pitting process is assessed through inspection programs, typically using various eddy current (EC) techniques, while the impact of pitting is minimized through deposit removal maintenance activities such as water lancing and chemical cleaning of SGs. This paper presents a probabilistic model of SG tube pitting corrosion that incorporates trends observed from a large EC inspection database from a nuclear generating station. The pitting occurrence process is modelled as a stochastic Poisson process and the pit size is treated as a random variable. The model is statistically calibrated with the available EC inspection data. The model is applied to estimate the probability of tube leakage, forced outage rate and the distribution of the number of tubes plugged per SG in a given operating interval. The proposed model is useful in optimizing strategies for the life-cycle management of SGs.


πŸ“œ SIMILAR VOLUMES


Corrosion of steam generator pipelines a
✍ V. Slugeň; J. Lipka; I. TΓ³th; J. Haőčík; Hinca; M. Lehota πŸ“‚ Article πŸ“… 2005 πŸ› Elsevier Science 🌐 English βš– 234 KB

The variability of the properties and the composition of the corrosion products of the stainless CrNi and mild steels in dependence on the conditions (temperature, acidity, etc.) is of such range that, in practice, it is impossible to determine the properties of the corrosion products for an actual