Preparation of superconducting molybdenum nitride fine powder by the plasma spraying method
β Scribed by R. Watanabe; I. Yazaki; Y. Igarashi; N. Toyota; K. Noto
- Publisher
- Springer
- Year
- 1986
- Tongue
- English
- Weight
- 280 KB
- Volume
- 5
- Category
- Article
- ISSN
- 0261-8028
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
In the preparation of Bi2CaSr2Cu20 x particles with an 80 K superconducting phase by an ultrasonic spray-pyrolysis method the particle size was changed from submicrometre to micrometre size by changing the concentration of the metal nitrates in the starting aqueous solution. The volume mean diameter
Ultra-fine amorphous powders in (Fe, Co, Ni)-B binary and ternary systems were produced by the chemical reduction method. The powders have a spherical shape with diameters ranging from 5 to 50 nm. The reaction consists mainly of the process of producing Me2B and Me(Me = Fe, Co, Nil. Fully dense bulk