## A bstra ct AI203-TiB 2 composites containing 0-50 wt% TiB 2 were prepared by sintering at 1600-1750Β°C ,for 15-120min in a vacuum. Relative density increased with TiB 2 addition from 97% (no TiB2) to about 99% ( lO-40wt% TiB2) on sintering at 1750Β°C Jbr 60 min. TiB 2 behaved as a sintering aid t
β¦ LIBER β¦
Preparation of Al2O3Ni composites by pressureless sintering in H2
β Scribed by W.H. Tuan; M.C. Lin; H.H. Wu
- Publisher
- Elsevier Science
- Year
- 1995
- Tongue
- English
- Weight
- 539 KB
- Volume
- 21
- Category
- Article
- ISSN
- 0272-8842
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Sintering and characterization of Al2O3-
β
Isao Kimura; Noriyasu Hotta; Yukio Hiraoka; Natsukaze Saito; Yuji Yokota
π
Article
π
1989
π
Elsevier Science
π
English
β 476 KB
Pressureless sintering of silicon nitrid
β
J.C. Almeida; A.T. Fonseca; R.N. Correia; J.L. Baptista
π
Article
π
1989
π
Elsevier Science
π
English
β 419 KB
Improving the mechanical properties of A
β
Kai Hui Zuo; Dong Liang Jiang; Qing Ling Lin; Yu-ping Zeng
π
Article
π
2007
π
Elsevier Science
π
English
β 783 KB
The (Al 2 O 3 + Ni) composite, (Al 2 O 3 + Ni)/Ni and Al 2 O 3 /(Al 2 O 3 + Ni)/Ni laminated materials were prepared by aqueous tape casting and hot pressing. Results indicated that the (Al 2 O 3 + Ni) composite had higher strength and fracture toughness than those of pure Al 2 O 3 . The fracture to
Sintering behaviour and microstructures
β
Z.H. Cai; D.L. Zhang
π
Article
π
2006
π
Elsevier Science
π
English
β 860 KB
Gel densification and ceramic sintering
β
Wenbang Zhang; F.P. Glasser
π
Article
π
1994
π
Elsevier Science
π
English
β 677 KB
Pressureless sintering of Si3N4 with Y2O
β
Pavol Ε ajgalΓk; Miroslav Haviar
π
Article
π
1992
π
Elsevier Science
π
English
β 393 KB