✦ Synopsis


Electrically conducting arachidic acid/polypyrrole (PPy) composite films were prepared by exposing the arachidic acid LB films containing ferric chloride to pyrrole vapor. The optimum conditions to deposit matrix LB film were the subphase temperature of 23-25"C, pH of 6.0 and ferric chloride concentration of 5.0 X M . The formation of PPy in the arachidic acid matrix LB films was confirmed by UV-visible spectra, FTIR spectra, and scanning electron micrographs. The average thickness of the composite LB films prepared at 0°C was 1525 A. The composite films prepared a t lower temperatures have more uniform surface and exhibit higher electrical conductivity than the films prepared a t higher temperatures do. The in-plain conductivity and the transverse conductivity of the composite film were 10-3-10-2 S/cm and S/cm, respectively, and, thus, the conductivity anisotropy was about lo3.


📜 SIMILAR VOLUMES


Preparation and electrical conductivity
✍ Yu Xu; Yunqi Liu; Jie Wu; Daoben Zhu 📂 Article 📅 1998 🏛 John Wiley and Sons 🌐 English ⚖ 299 KB 👁 2 views

Five poly(3-alkylthiophene) s (P3ATs) with different alkyl side chains were synthesized. Pure P3ATs alone are not well suited for manipulation by the Langmuir-Blodgett (LB) technique, but their mixed systems with arachidic acid can be used to prepare high-quality Y-type films with the vertical dippi

Conducting Composites of Polyurethane Re
✍ Hüseyin Deligöz; Bernd Tieke 📂 Article 📅 2006 🏛 John Wiley and Sons 🌐 English ⚖ 176 KB

## Abstract **Summary:** Three methods were used for solvent‐free preparation of conducting composites of PUR and PPy. In all cases, PUR was prepared from TDI and hydroxol 15‐W as polyol cross‐linker, whereas PPy was obtained upon oxidative coupling of Py using ferric chloride as oxidant. In method

Preparation and characterisation of Lang
✍ O. Szczur; R. W. Munn 📂 Article 📅 1999 🏛 John Wiley and Sons 🌐 English ⚖ 249 KB 👁 2 views

Langmuir films of the title compound have been spread on an aqueous subphase at various values of pH at 10, 15 and 20 8C. Increasing pH and increasing temperature favour stable films, but at the higher subphase pH and temperature values the pressure-area isotherms exhibit a transition to aggregated