𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Preparation and characterization of temperature-sensitive poly(N-isopropylacrylamide)-g-poly(L-lactide-co-ε-caprolactone) nanofibers

✍ Scribed by Sung In Jeong; Young Moo Lee; Joohyeon Lee; Young Min Shin; Heungsoo Shin; Youn Mook Lim; Young Chang Nho


Publisher
The Polymer Society of Korea
Year
2008
Tongue
English
Weight
651 KB
Volume
16
Category
Article
ISSN
1598-5032

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Characterization, degradation, and mecha
✍ Hanna Bramfeldt; Pierre Sarazin; Patrick Vermette 📂 Article 📅 2007 🏛 John Wiley and Sons 🌐 English ⚖ 300 KB

## Abstract A series of three biocompatible P(CL‐__co__‐LA)‐PEG‐P(CL‐__co__‐LA) copolymers were synthesized using ring‐opening polymerization and characterized by ^1^H‐NMR, gel permeation chromatography, DSC, dynamic‐mechanical analysis, and X‐ray diffraction. The number of monomer units was kept c

Preparation and characterization of poly
✍ Jin Zhao; Xiaoyan Yuan; Yuanlu Cui; Quanbo Ge; Kangde Yao 📂 Article 📅 2003 🏛 John Wiley and Sons 🌐 English ⚖ 530 KB

## Abstract Polyblend fibrous scaffolds in mass ratios of 100/0, 90/10, 80/20, and 70/30 from poly(L‐lactide) (PLLA) and poly(ϵ‐caprolactone) (PCL) for cartilage tissue engineering were prepared in three steps: gelation, solvent exchanging, and freeze‐drying. Effects of the blend ratio, the exchang

Characterization of the mechanical and t
✍ V. Vilay; M. Mariatti; Zulkifli Ahmad; K. Pasomsouk; Mitsugu Todo 📂 Article 📅 2009 🏛 John Wiley and Sons 🌐 English ⚖ 973 KB

## Abstract Two series of biodegradable polymer blends were prepared from combinations of poly(L‐lactide) (PLLA) with poly(ϵ‐caprolactone) (PCL) and poly(butylene succinate‐__co__‐L‐lactate) (PBSL) in proportions of 100/0, 90/10, 80/20, and 70/30 (based on the weight percentage). Their mechanical p

Enhanced crystallization of poly(L-lacti
✍ Hideto Tsuji; Akira Mizuno; Yoshito Ikada 📂 Article 📅 2000 🏛 John Wiley and Sons 🌐 English ⚖ 193 KB 👁 1 views

Copolymer of L-lactide and -caprolactone [P(LLA-CL)] (50/50) was synthesized using stannous octoate and was stored at room temperature. The change in physical properties occurring during this storage at room temperature was investigated by differential scanning calorimetry (DSC), X-ray diffractometr