๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Point Defects in highly deformed vanadium

โœ Scribed by Anand, M. S. ;Pande, B. M. ;Agarwala, R. P.


Publisher
John Wiley and Sons
Year
1973
Tongue
English
Weight
259 KB
Volume
17
Category
Article
ISSN
0031-8965

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Recovery of point defects in iron after
โœ L.J. Cuddy ๐Ÿ“‚ Article ๐Ÿ“… 1968 ๐Ÿ› Elsevier Science โš– 550 KB

High-purity iron was severely deformed at 77ยฐK by rolling or drawing under liquid nitrogen. Changes in electrical resist.ivity were used to measure the recovery during isochronal and isothermal anneals in the temperature range llO-520ยฐK. A sharp recovery stage was observed at 211ยฐK for which t,he ac