✦ LIBER ✦
Plastic deformation analysis in machining of Inconel-718 nickel-base superalloy using both experimental and numerical methods
✍ Scribed by Abdul B. Sadat; Mohan Y. Reddy; B.P. Wang
- Publisher
- Elsevier Science
- Year
- 1991
- Tongue
- English
- Weight
- 802 KB
- Volume
- 33
- Category
- Article
- ISSN
- 0020-7403
No coin nor oath required. For personal study only.