Pitting corrosion of stainless steel in water-organic solvent mixtures: II
โ Scribed by B.A. Abd-El-Nabey; N. Khalil; M.M. Eisa
- Publisher
- Elsevier Science
- Year
- 1984
- Weight
- 251 KB
- Volume
- 22
- Category
- Article
- ISSN
- 0376-4583
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
## Abstract On a costโperformance basis, superferritic stainless steel (SFSS) grades can now be considered competitive choices for brackish and sea water cooling systems. The pitting corrosion of a SFSS (X2CrNiMoTi 25 3.6 3.5) was tested in a chloride/sulfate solution similar to sea water, as a fun
## Abstract In the temperature range from 6 to 40ยฐC the temperature dependence of pitting corrosion may be expressed by the Artheniusโequation. The lowering of the breakdown potential in this range shows a linear dependence on the reziprokal value of the absolute temperatur. From the temperature de
## Abstract A literature survey has lead to the conclusion that a theory which postulates an increased anodic reactivity on a local site in the passive film is very probable. Experiments have been set up to confirm these suggestions. By means of the electronโmicroanalyser, it is shown that CI^โ^ion