𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Pitting corrosion of copper in sulphate solutions: inhibitive effect of different triazole derivative inhibitors

✍ Scribed by W. Qafsaoui; Ch. Blanc; J. Roques; N. Pébère; A. Srhiri; C. Mijoule; G. Mankowski


Book ID
111532255
Publisher
Springer
Year
2001
Tongue
English
Weight
153 KB
Volume
31
Category
Article
ISSN
0021-891X