𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Pitting and galvanic corrosion behavior of stainless steel with weld in wet-dry environment containing CI−

✍ Scribed by Lin Cui; Li Xiaogang; Dong Chaofang


Book ID
117695434
Publisher
Chinese Electronic Periodical Services
Year
2007
Tongue
English
Weight
864 KB
Volume
14
Category
Article
ISSN
1005-8850

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Pitting corrosion behavior of superferri
✍ G. Moretti; G. Quartarone; A. Tassan; A. Zingales 📂 Article 📅 1993 🏛 John Wiley and Sons 🌐 German ⚖ 674 KB

## Abstract On a cost‐performance basis, superferritic stainless steel (SFSS) grades can now be considered competitive choices for brackish and sea water cooling systems. The pitting corrosion of a SFSS (X2CrNiMoTi 25 3.6 3.5) was tested in a chloride/sulfate solution similar to sea water, as a fun

Hydrogen permeation behavior and corrosi
✍ C. Zheng; Y. Huang; C. Huo; Q. Yu 📂 Article 📅 2007 🏛 John Wiley and Sons 🌐 German ⚖ 190 KB

## Abstract Hydrogen permeation of 16Mn steel under a cyclic wet–dry condition was investigated by Devanathan–Stachurski's electrolytic cell with a membrane covered on the exit side by a nickel layer and the weight loss was measured for each wet–dry cycle. The results show that hydrogen permeation