๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Physical Behavior of Nanoporous Anodic Alumina Using Nanoindentation and Microhardness Tests

โœ Scribed by Te-Hua Fang; Tong Hong Wang; Chien-Hung Liu; Liang-Wen Ji; Shao-Hui Kang