Oxidation-sulfidation behavior of nickel-base superalloys and MCrAl coatings

✍ Scribed by K. Natesan


Publisher
Elsevier Science
Year
1987
Weight
933 KB
Volume
87
Category
Article
ISSN
0025-5416

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Oxidation behavior of CrNx and (Cr,Al)Nx
✍ S. Hofmann; H. A. Jehn 📂 Article 📅 1990 🏛 John Wiley and Sons 🌐 German ⚖ 525 KB

## Abstract Reactively magnetron‐sputtered CrN~x~ and (Cr,Al)N~x~ hard costings were oxidized in air at temperatures between 500°C and 900°C for periods up to 16 h. The original and the oxidized samples were characterized by scanning electron microscopy, X‐ray diffraction and scanning Auger electro