Oxidation kinetics of microcrystalline Ni–11.5Cr–4.5Co–0.5Al superalloy sheet fabricated by electron beam physical vapor deposition at 900 °C

✍ Scribed by Gang Zeng; Mingwei Li; Jiecai Han; Xiaodong He; Wenzheng Li