๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Oxidation behavior of a single-crystal Ni-base superalloy in air at 900, 1000 and 1100

โœ Scribed by L. Huang; X. F. Sun; H. R. Guan; Z. Q. Hu


Publisher
Springer US
Year
2007
Tongue
English
Weight
120 KB
Volume
27
Category
Article
ISSN
1023-8883

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Anisothermal creep behavior at very high
โœ J. Cormier; X. Milhet; J. Mendez ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 438 KB

Nickel-based superalloy single crystal specimens have been tested under anisothermal creep conditions using two different routes, both including an overheating stage. In the first route, the material is tested under creep conditions at 1050 โ€ข C, then submitted to an overheating regime at 1200 โ€ข C, a