## Abstract Growth kinetics of zinc (tris) thiourea sulphate (ZTS) crystals investigated as a function of supersaturation is reported in this communication. Crystal growth rates were investigated normal to the (100), (010) and (001) faces under growth conditions employed for bulk crystal growth. Th
Optical imaging of the growth kinetics and polar morphology of zinc tris(thiourea) sulphate single crystals
β Scribed by S. Dinakaran; S. Verma; S. Jerome Das; S. Kar; K. S. Bartwal
- Publisher
- John Wiley and Sons
- Year
- 2010
- Tongue
- English
- Weight
- 293 KB
- Volume
- 45
- Category
- Article
- ISSN
- 0232-1300
No coin nor oath required. For personal study only.
β¦ Synopsis
Abstract
Growth kinetics of zinc tris(thiourea) sulphate (ZTS) single crystals was imaged in two different growth geometries using laser shadowgraphy technique. Growth rates of the {010} and {001} faces were computed as a function of supersaturation. The time evolution of polar morphology of ZTS crystal based on the growth rates is presented. Except (00$ \bar 1 $) face, all the other three faces are found to have a dead zone resulting in large induction period of growth. The anisotropy in the growth rates of the (001) and (00$ \bar 1 $) faces was very high, resulting in polar morphology. Different chemical environments on two sides of the (001) slice are suggested as the possible cause for the polar morphology of the crystals. (Β© 2010 WILEYβVCH Verlag GmbH & Co. KGaA, Weinheim)
π SIMILAR VOLUMES
## Abstract Optical absorption of tris thiourea zinc sulphate (ZTS) single crystals has been measured and its direct band gap was found to be 3.6 eV. Theoretical calculations were carried out to determine the linear optical constants such as extinction coefficient and refractive index. Further the
## Abstract Tris (thiourea) zinc sulphate (ZTS), a semiorganic nonlinear optical (NLO) material has been synthesized at 30 Β°C. The solubility was determined in different solvents such as water, ethanol and water mixture of ethanol (1:1). Good quality single crystals with size 10 Γ 8 Γ 6 mm^3^ were
Nucleation parameters such as metastable zone width, induction period and interfacial energy have been determined for the aqueous solution growth of bis thiourea cadmium acetate (BTCA) single crystals. Solubility of BTCA has been determined for various temperatures. Metastable zone width and inducti