The change in resistivity, on plastic de
β
W.H Aarts; R.K Jarvis
π
Article
π
1954
π
Elsevier Science
β 384 KB
Wires of silver, gold, and copper and some silver-copper and silver-gold alloys were stretched at room temperature, -80Β°C and at the liquid air point. The change of resistivity was determined as well as the recovery of resistivity on warming from the low temperatures to room temperature. The silver-