𝔖 Bobbio Scriptorium
✦   LIBER   ✦

On the characterization by shrinkage forces of as-spun poly(ethylene terephthalate) filaments

✍ Scribed by Ch.D. Bechev


Publisher
Elsevier Science
Year
1995
Tongue
English
Weight
496 KB
Volume
14
Category
Article
ISSN
0142-9418

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


The effect of carriers on drawn poly(eth
✍ W. Ingamells; A. M. Yabani πŸ“‚ Article πŸ“… 1978 πŸ› John Wiley and Sons 🌐 English βš– 440 KB πŸ‘ 2 views

## Abstract The effect of various organic compounds on the birefringence equilibrium shrinkage and swelling of poly(ethylene terephthalate) filaments was studied. Evidence is presented that suggests the carrier action of the compounds is dominated by dispersion forces and that interaction between d

Effect of initial take-up speed on prope
✍ J. F. Hotter; J. A. Cuculo; P. A. Tucker; B. K. Annis πŸ“‚ Article πŸ“… 1998 πŸ› John Wiley and Sons 🌐 English βš– 426 KB πŸ‘ 2 views

The effect of initial take-up speed on the properties and structure of both as-spun and drawn/heat-set poly(ethylene terephthalate) filaments was characterized through measurements of birefringence, percent crystallinity, tensile properties, high temperature shrinkage, loss tangent temperature depen

Effect of liquid isothermal bath positio
✍ J. F. Hotter; J. A. Cuculo; P. A. Tucker; B. K. Annis πŸ“‚ Article πŸ“… 1998 πŸ› John Wiley and Sons 🌐 English βš– 445 KB πŸ‘ 2 views

The ability to produce as-spun poly(ethylene terephthalate) (PET) filaments that possess previously unsurpassed levels of as-spun orientation and tensile properties was achieved through the implementation of a device described as a liquid isothermal bath (LIB). Although much has been published regar

Effect of winding speed on the physical
✍ H. M. Heuvel; R. Huisman πŸ“‚ Article πŸ“… 1978 πŸ› John Wiley and Sons 🌐 English βš– 917 KB

## Abstract As‐spun fibers of poly(ethylene terephthalate), PET, made at winding speeds ranging from 2000 to 6000 m/min exhibit quite different physical structures. Yarns wound at relatively low speeds are amorphous, whereas those spun at high speeds contain well‐developed crystals of closely packe