Nuclear techniques for bulk and surface analysis of materials

โœ Scribed by M. D. D'Agostino; E. A. Kamykowski; F. J. Kuehne; G. M. Padawer; E. J. Schneid; R. L. Schulte; M. C. Stauber; F. R. Swanson


Book ID
112765863
Publisher
Springer
Year
1978
Tongue
English
Weight
966 KB
Volume
43
Category
Article
ISSN
1588-2780

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Comparative electron spectroscopy for ch
โœ T.L. Barr ๐Ÿ“‚ Article ๐Ÿ“… 1995 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 536 KB

In adsorption and catalytic technology, it is often suggested that many key high-surface area materials, e.g. zeolites, are "all surface". Despite this contention numerous examples have recently been found employing comparative solidstate magic-angle spinning nuclear magnetic resonance (MAS NMR; bul